S4S, Rough, and Board Feet: How Lumber Is Sold
Learn how lumber is sold: S4S, S2S, rough, nominal vs actual dimensions, hardwood quarters, board feet, grades, and how to pick boards at the rack.
Lumber is sold in a language of abbreviations and historical conventions that often confuse even experienced woodworkers. The difference between rough sawn lumber and S4S lumber, the meaning of a board foot, and why a nominal 2x4 is not 2 inches by 4 inches are all practical matters that affect what you buy and how you use it. This guide explains the terms and the judgement needed when selecting boards at the rack.
Rough, S2S, and S4S: What the Surface Tells You
Rough lumber has been sawn and dried but not planed or edged. The surfaces are textured with saw marks, and the edges may be uneven. Rough lumber is typically thicker than its nominal dimension to allow for flattening and squaring. For example, a 4/4 rough board is often 1 inch thick, giving enough material to remove warp and arrive at a finished 3/4 inch thickness.
S2S means surfaced two sides: the two broad faces have been planed flat and parallel, but the edges remain rough. This is common for lumber that will be ripped or jointed by the woodworker.
S4S means surfaced four sides: both faces and both edges are planed and squared. S4S lumber is ready for use in projects that require consistent dimensions, such as cabinet parts, trim, and furniture components. It is also the form most commonly sold in home centers. The trade-off is that S4S lumber has less thickness for future flattening; if it cups or twists later, there may not be enough material to true it again. If the milling and finishing work adds up to more than the project is worth, consider browsing ready-made home office furniture collections instead of building from scratch.
Nominal vs Actual Dimensions
The dimensions used to sell lumber are nominal, not actual. A nominal 1x4 is actually 3/4 inch by 3-1/2 inches (19 mm by 89 mm). A nominal 2x4 is 1-1/2 inches by 3-1/2 inches (38 mm by 89 mm). This convention comes from the rough green size before drying and planing. When planning a project, always design around actual dimensions, not nominal ones. The difference can accumulate across multiple pieces and throw off a layout.
Hardwood thickness is sold in quarters, referring to the rough thickness in quarter-inches. 4/4 is one inch rough, often surfacing to 3/4 inch (19 mm). 8/4 is two inches rough, typically finishing at 1-3/4 inches (44 mm). Other common thicknesses are 5/4, 6/4, and 12/4. The quarter system allows buyers to specify the rough thickness they need for a project, with the understanding that milling will reduce it.
The Board Foot: A Volume, Not a Length
Hardwood lumber is often sold by the board foot, a unit of volume equal to 144 cubic inches. One board foot is 12 inches by 12 inches by 1 inch thick (305 mm by 305 mm by 25 mm), or any equivalent volume. The formula for calculating board feet is:
(Thickness in inches × Width in inches × Length in inches) ÷ 144 = Board feet
For rough lumber, thickness is the nominal quarter thickness (e.g., 1 inch for 4/4). Width and length are measured in inches. For example, a board 1 inch thick, 6 inches wide, and 8 feet long (96 inches) contains 4 board feet. When buying S4S lumber, the board foot is still used, but the calculation uses the actual surfaced dimensions. Some retailers sell S4S by the linear foot instead, so clarify the unit before ordering.
Hardwood Grades: What They Describe
Hardwood grades are assigned by rules established by the National Hardwood Lumber Association (NHLA). The grade describes the proportion of clear, defect-free cuttings that can be obtained from a board, not its overall appearance. Higher grades (FAS, Select) yield longer and wider clear cuttings, while lower grades (No. 1 Common, No. 2 Common) contain more knots, checks, and other defects. The grade does not indicate strength or durability; it is a measure of yield for a specific use. For painted projects, a lower grade may be perfectly adequate; for fine furniture with exposed surfaces, a higher grade reduces waste.
Kiln-Dried vs Air-Dried
Kiln-dried lumber has been dried in a controlled environment to a specific moisture content, typically 6-8% for interior use. This process reduces the risk of shrinkage and movement after milling. Air-dried lumber has been stacked and dried naturally, which takes longer and may leave a higher moisture content, often 12-15% or more depending on climate. Air-dried lumber is suitable for outdoor projects or where some movement is acceptable, but for interior furniture, kiln-dried stock is preferred. Always check moisture content with a meter before milling, especially if the lumber has been stored in an uncontrolled environment.
Selecting Boards at the Rack
When picking lumber, inspect each board for defects that will affect its use. Twist, cup, bow, and crook are common distortions. Twist is a helical warp along the length; sight down the board to detect it. Cup is a concave or convex curvature across the width; place a straightedge across the face. Bow is a curve along the length of the face; sight down the edge. Crook is a curve along the edge. Some defects can be removed during milling, but excessive warp may leave insufficient thickness.
Checks are cracks that run along the grain, often at the ends of boards. They can deepen after drying and may not be visible until the board is cut. Pith is the soft, spongy core at the center of the log; boards containing pith are more prone to checking and movement. Avoid boards with pith if the project requires stability.
Also look for knots, which are acceptable in some applications but can dull tools and weaken the board. Decide based on the project: a knot in a painted shelf may be fine, but in a structural component it may not.
When to Choose Rough, S2S, or S4S
| Option | Choose when | Avoid when |
|---|---|---|
| Rough | You have a jointer and planer and want maximum thickness for custom milling. | You lack milling equipment or need ready-to-use stock. |
| S2S | You plan to rip or joint edges yourself but want flat faces. | You need finished edges without further machining. |
| S4S | You need consistent, ready-to-use dimensions for cabinet parts, trim, or small projects. | You require thick stock for resurfacing or structural use. |
Moisture Content and Movement
Wood moves as it gains or loses moisture. Kiln-dried lumber is more stable, but even it will expand and contract with seasonal humidity changes. Design joints with allowance for movement, especially in wide panels. Air-dried lumber may continue to dry after purchase, leading to shrinkage and warping. If using air-dried stock, acclimate it in the shop before milling and monitor moisture content.
Board Foot Calculation in Practice
To calculate board feet for a stack of lumber, measure each board’s thickness (in quarters for rough, or actual inches for S4S), width in inches, and length in inches. Multiply and divide by 144. For multiple boards, sum the board feet. When buying, ask whether the price is per board foot or per linear foot; the two are not interchangeable. For rough lumber, the board foot is based on the nominal rough dimensions, not the finished size.
Related Guides
For a step-by-step process of milling rough lumber into flat, square stock, see the guide to milling rough lumber. For information on how different species behave and which to choose for a project, see the wood species guide.
Common questions
What does S4S mean in lumber?
S4S stands for surfaced four sides. It means the lumber has been planed on both faces and both edges to create flat, parallel surfaces and square edges. S4S lumber is ready for use in projects that require consistent dimensions, but it has less thickness for future flattening than rough lumber.
How do you calculate board feet?
Multiply thickness in inches by width in inches by length in inches, then divide by 144. For rough lumber, use the nominal thickness (e.g., 1 inch for 4/4). For S4S lumber, use the actual surfaced dimensions. The result is the volume in board feet.
Why is a 2x4 not 2 inches by 4 inches?
The nominal dimensions refer to the rough green size before drying and planing. A nominal 2x4 is dried and planed down to 1-1/2 inches by 3-1/2 inches (38 mm by 89 mm). Always design projects using actual dimensions.
What is the difference between kiln-dried and air-dried lumber?
Kiln-dried lumber is dried in a controlled environment to a low moisture content, typically 6-8%, making it more stable for interior use. Air-dried lumber dries naturally and may have a higher moisture content, often 12-15% or more, so it is more prone to movement and is better suited for outdoor projects or where some shrinkage is acceptable.
How do you identify defects like twist or cup when buying lumber?
Sight down the length of the board to detect twist, which appears as a helical warp. To check for cup, place a straightedge across the width; a gap indicates cupping. Bow is visible by sighting down the face, and crook by sighting down the edge. Also inspect for checks (cracks) and pith (soft center) which can cause instability.
Read next
- Milling Rough Lumber: Flat, Square, and In Order The fixed order for milling rough lumber: one face flat, one edge square, then thickness and width. Why a planer alone cannot flatten a board.
- Resawing Lumber on a Band Saw: Technique and Judgement Cut boards through thickness into thinner stock for bookmatching and veneer. Blade choice, tension, fence setup, drift, and why resawn boards cup.
- Edge Joining Boards for a Tabletop How to edge join boards for a tabletop: jointing edges, grain and ring orientation, glue-up pressure, cauls, and flattening after the panel comes out of the clamps.
- How to Make a Cutting Board: Edge Grain and End Grain Learn to make a cutting board with step-by-step instructions. Covers wood selection, glue-up, clamping, and food-safe finish. Avoid common mistakes.
- Scarf Joint: Joining Boards End to End A scarf joint joins two boards end to end along a long bevel so glue meets long grain. Covers plain and hooked scarfs, hand and machine cutting, fit, and failure.